Answers are grounded in this paper and cite their sources.
N‐type Mg3.2Sb1.5Bi0.5 materials are prepared by cation‐site doping with lanthanides (La, Ce). Both La‐ and Ce‐doped samples exhibit a higher doping limit and greater efficiency than those of chalcogen (Te, Se, S)‐doped n‐type Mg3.2Sb1.5Bi0.5 samples. High electron carrier concentration ≈9 × 1019 cm−3 is obtained in Mg3.18La0.02Sb1.5Bi0.5 and Mg3.185Ce0.015Sb1.5Bi0.5, which is close to the theoretical doping‐concentration limit and induces contributions from more electron bands. A higher electrical conductivity was thus obtained and is beneficial to the enhanced ZT values for lanthanide‐doped Mg3.2Sb1.5Bi0.5. The highest ZT value ≈1.6 is achieved in Mg3.19La0.01Sb1.5Bi0.5 at 693 K, along with a ZT ≈1.50 in Mg3.19Ce0.01Sb1.5Bi0.5 at 693 K, indicating that lanthanides provide a promising doping strategy for Mg3.2Sb1.5Bi0.5‐based materials.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: