Inhibition of cubic‐rhombohedral phase transformation and low‐temperature sintering at 1000°C were achieved for 10‐mol%‐Sc 2 O 3 ‐doped cubic‐ZrO 2 by the presence of 1 mol% Bi 2 O 3 . The powders of 1‐mol%‐Bi 2 O 3 –10‐mol%‐Sc 2 O 3 ‐doped ZrO 2 were prepared using a hydrolysis and homogeneous precipitation technique. No trace of rhombohedral‐ZrO 2 phase could be detected, even after sintering at 1000°–1400°C. The average grain size of the ZrO 2 sintered at 1200°C was >2 μm because of grain growth in the presence of Bi 3+ . Cubic, stabilized Bi‐Sc‐doped ZrO 2 sintered at 1200°C had sufficient conductivity at 1000°C (0.33 S/cm) to be used as an electrolyte for a solid‐oxide fuel cell (SOFC) and at 800°C (0.12 S/cm) for an intermediate‐temperature SOFC.