AIM: The purpose of this study was to compare the marginal and internal fit of Co-Cr and titanium ceramic crowns fabricated with 2 different techniques: CAD/CAM milling and traditional casting (TC). MATERIALS AND METHODS: Ten traditional casting of Co-Cr (TCC), 10 CAD/CAM milling of Co-Cr (MC), 10 traditional casting of titanium (TCT), 10 CAD/CAM milling of titanium ceramic crowns (MT) were fabricated. Silicone replicas were obtained to measure internal gap volume, marginal gap and internal adaptation that was evaluated at 3 regions: axial wall, axio-occlusal angle, and occlusal surface. Measurements were made with a X-ray micro computerized tomography (micro-CT) and analyzed with Bonferroni and Dunnet T3 post-hoc tests (α = 0.05). RESULTS: for MT. Mean internal gap volume values MT group were smaller than those of groups but only statistically not significant for TCC group (P > 0.05). CONCLUSION: All groups performed similar marginal adaptation. The cement film thickness at axio-occlusal angle point and occlusal region were higher for MC crowns.
No takes yet. Share an insight, caveat, or question.
Tamaç et al. (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: