Answers are grounded in this paper and cite their sources.
The electrical resistivity of irons containing different levels of impurity have been measured at 77° and 293°K for a range of grain sizes. The resistivity of a given iron is found to vary with the grain diameter (d mm) as ρ = A+B log(1/d). A and B are both temperature dependent, increasing with increasing temperature. With increasing impurity content, the parameter A increases and B decreases. Thus the purer iron shows a larger variation of resistivity with grain size than the less pure material. The observed relationship can only be explained in terms of a grain-boundary scattering process if the effective width of the boundaries is much greater than is usually believed.
No takes yet. Share an insight, caveat, or question.
Braunović et al. (1969) studied this question.