In this study influence of compaction pressure, sintering temperature, and sintering time on mechanical and wear behavior of the fly ash reinforced copper-based composites are analyzed. The composites were prepared by powder metallurgy (P/M) technique with copper as matrix, 5 and 10 wt% of fly ash as reinforcement. The green compacts were prepared at three different pressures such as 350, 400, and 450 MPa. The prepared green composites were sintered at 700, 800, and 900 °C for the time period of 30, 60, and 90 min, respectively. From the results it is observed that when the process parameter increases the density, hardness, compression strength, and wear resistance increases.