The 0‐3 type CaBi 4 Ti 4 O 15 :30 wt%BiFeO 3 composite shows much better high‐temperature piezoelectric properties than the single‐phase CaBi 4 Ti 4 O 15 or BiFeO 3 ceramics. The composite with 0‐3 type connectivity exhibits a high density of 7.01 g/cm 3 , a saturated polarization of 21.5 μC/cm 2 and an enhanced piezoelectric d 33 of 25 pC/N. After the poled composite was annealed at 600°C, its d 33 is 21 pC/N at room temperature. Resistance of the composite decreases slowly from 10 9 ohm at 20°C to ~10 5 ohm at 500°C. Furthermore, the poled composite shows strong radial and thickness dielectric resonances at 20°C‐500°C.