Eu-doped and undoped polycrystalline Ca10(PO4)OH2 hydroxyapatite [1] were synthesized by using the chemical-precipitation technique [1].Chemical composition of the samples was confirmed by using Inductively Coupled Plasma (ICP) spectroscopy.The multi-methodological characterization achieved through powder X-Ray diffraction (PXRD) and photoluminescence (PL) techniques, showed that the Eu entered in Ca1 site in the dried (120 °C) doped samples and in those calcinated (450 °C) at low temperature: these samples show low crystallinity, good luminescence and very low crystallite size.On the contrary, Eu-doped sample calcinated at 900°C showed very high crystallinity, with a crystallite size of 148 nm, while PL spectroscopy suggested that this sample presents the highest and narrowest emission bands.Specifically, the PL emissions peak at 573 nm, corresponding to the 5 D0-7 F0 of the Eu 3+ transition in Ca2 site, was more than 10 times more intense than the emission peak at 592 of Eu 3+ in Ca1 site, indicating the complete migration of Eu 3+ ions in the Ca2 sites of HAp framework for the high temperature sample.FTIR and Raman spectra showed slight band shifts with increasing annealing temperature of the samples.Results show that low crystalline HAp obtained at 120° and 450°, could be employed as luminescent drug carriers, while high crystalline HAp, annealed at 900°, could be suitable materials for biological optical imaging [2].
No takes yet. Share an insight, caveat, or question.
Mele et al. (2023) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: