Extended defects formed by high-fluence helium implantation in silicon have been studied as a function of the implantation temperature, from room temperature up to 800 °C. Transmission electron microscopy results show that the formation of cavities created by a 50 keV He implantation with a fluence of 5×1016 cm−2 can be divided into three stages. For implantation temperature up to about 300 °C the bubble size is relatively constant but the bubble density decreases due to the increase in dynamic annealing. Above 300 °C, where divacancies are no longer stable and when the helium is mobile, both the density and size of the cavities stay relatively constant. In this stage, helium starts to diffuse out and the cavities become more and more faceted as the temperature increases. Concurrently interstitial-type defects appear: small elongated rod-like defects at relatively low temperatures and large ribbon-like defects at 600 °C. Finally, for implantation at 800 °C, no cavities are formed and only dislocation loops and {113}’s (ribbon-like defects and rod-like defects), are observed depending on the deposited energy profile. At this temperature the defect annealing during implantation becomes efficient to convert ribbon-like defects into dislocation loops.
No takes yet. Share an insight, caveat, or question.
David et al. (2003) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: