Thin films of Bi2VO5.5 have been prepared epitaxially using a pulsed-laser deposition method on a Si(100) substrate using TiN as a buffer layer and SrTiO3 as a seed layer. The films have smooth surface morphology with atomically flat terraces and steps of 4 Å in height. The ferroelectric characterization shows a spontaneous polarization of 2.2 μC/cm2 and a coercive field (Ec) of 22 kV/cm. The leakage current obtained is about 5×10−6 A/cm2 at a drive voltage of ±2 V.