Inconel 718 is a typical alloy suitable for selective laser melting (SLM) method.The fabrication parameters have determined effect on the mechanical properties of the produced parts.The effects of laser power and scanning speed on the microstructure and mechanical properties of the fabricated bars of Inconel 718 alloy were investigated.With the increase of laser power and decrease scanning speed, the stacking of melt pools came to be in order, less pores appeared and mechanical properties increased.Lase energy density (laser power divided by scanning speed) is in positive relationship with the mechanical properties.At the combination of 200W and 1000mm/s or combination of 150W and 500mm/s best mechanical properties with yield strength of 775MPa, ultimate tensile strength of 1055MPa and elongation of 29.5% were achieved.But, for the same laser energy density, the variation of laser power has more significant effect on the pore defect than that of scanning speed.
No takes yet. Share an insight, caveat, or question.
Jinwu Kang (2019) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: