Answers are grounded in this paper and cite their sources.
The spark plasma sintering (SPS) technique is applied in combination with the hydrogen decrepitation process for the recycling of SmCo5magnets. The SmCo5magnets for recycling were first decrepitated by hydrogen gas at a pressure of 4 bar for 3 h to produce decrepitated powder. This powder was then used to prepare isotropic sintered magnets using the SPS technique by sintering at 800 °C-1000 °C for 1 min. Full densification of the SPS magnets was possible at a temperature of 1000 °C. The sample that was sintered at 900 °C showed the best internal coercivity (iHc) of higher than 1500 kA/m with a high remanence (Br) value of 0.47 T and energy product (BHmax) of 43.4 kJ/m3. The properties of the SPS sample sintered at 900 °C are compared to the conventionally sintered (CVS) sample prepared by using fresh SmCo5powder. The results show an improvement in the magnetic properties of the SPS sample in comparison to the CVS sample at room temperature, and the possibility to use the SPS sample at a high temperature of 180 °C, where the sample showed good magnetic properties ofiHcof 1502 kA/m,Brof 0.44 T, andBHmaxof 36.4 kJ/m3. Microstructure and X-ray diffraction patterns of the SPS and the CVS samples show that they consist of a SmCo5matrix with Sm2Co7and Sm oxides.
No takes yet. Share an insight, caveat, or question.
Awais Ikram (2018) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: