The long-term high-temperature oxidation behavior of Ni-based superalloy GH4169 was investigated at 900 °C for 10–2000 h, and its oxidation mass-gain kinetics approximately followed a parabolic law. After oxidation, the cross-section of the alloy exhibited a three-layer structure: the oxide layer was loose and porous, consisting primarily of Cr 2 O 3 , TiO 2 , NiO, Nb 2 O 5 , MoO 3 and NiCr 2 O 4 spinel; the internal oxidation region was dense and contained numerous elongated TiO 2 –Al 2 O 3 duplex oxides, with a Cr-depleted layer formed at its top; and NbC carbides precipitated in the substrate. The oxidation of the alloy was mainly governed by the diffusion of Cr, Al, Ti, Nb, Ni and O. During high-temperature oxidation, the inhomogeneous growth of TiO 2 promoted the formation of surface defects and intragranular cracks. Based on the coupled oxygen diffusion and interfacial reaction mechanism, a numerical model was established to predict the coordinated thickening of the external oxide layer and internal oxidation region and simulate the growth stress evolution. The calculated growth stress was mainly concentrated in the external oxide layer, and its maximum equivalent value increased from approximately 656 MPa at 10 h to 1410 MPa at 2000 h.
No takes yet. Share an insight, caveat, or question.
Zuo et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: