Although BaLiF 3 ceramic has a high quality‐factor at microwave frequencies ( Q × f value = ∼83000 GHz) coupled with a low sintering temperature (750°C/2 h), its high negative temperature coefficient of resonant frequency ( τ f = ∼ −70 ppm/°C) prevents practical applications. In the present paper, we employed SrTiO 3 as a second phase (7 mol%) to tune the negative τ f value to near zero (∼2.5 ppm/°C) and added a small amount of LiF (4 mol%) to reduce the sintering temperature to ∼800°C. Sintering in the N 2 atmosphere has a beneficial effect on the density, while it has a detrimental impact on the Q × f value of the sintered body due to the partial reduction of Ti 4+ in the SrTiO 3 (SrTi 4+ 1‐ x Ti 3+ x O 3‐ x F x ) and F‐vacancies in the BaLiF 3 (BaLiF 3‐x ) . The 0.93BaLiF 3 +0.07SrTiO 3 composite with 4 mol% LiF addition exhibits excellent combined microwave dielectric properties ( ε r = 14, Q × f = 55 000 GHz, and τ f = −3 ppm/°C), coupled with low sintering temperature (785°C/3 h) and good cofiring chemical compatibility with silver, which is a promising candidate for LTCC applications.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Zheng et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: