The low thermal conductivity and high toughness are key indicators for long‐life thermal barrier coatings (TBCs), and inducing a second phase is a good way to boost these properties. To address the high thermal conductivity and low fracture toughness of NdAlO 3 , NdAlO 3 ‐x wt.% NdTaO 4 (x = 5, 10, 15, and 20) dual‐ferroelastic composite ceramics are designed and fabricated. With the introduction of NdTaO 4 , the fracture toughness increased from 1.97 ± 0.13 MPa·m 1/2 of NdAlO 3 to 2.88 ± 0.13 MPa·m 1/2 of NdAlO 3 ‐20 wt.% NdTaO 4 composite, representing an improvement of more than 46%. The enhancement in toughness is attributed to the dual‐ferroelastic toughening mechanism, wherein crack propagation is deflected by domain boundaries, and domain switching and crack bridging collectively dissipate fracture energy to enhance toughness. The thermal conductivity decreases from 3.55 W·m −1 ·K −1 of NdAlO 3 to 2.97 W·m −1 ·K −1 of NdAlO 3 ‐20 wt.% NdTaO 4 composite at 900°C, corresponding to a reduction of 16%. Moreover, the thermal expansion coefficients (TECs) reach 11.68 × 10 −6 K −1 at 1200°C. This study demonstrates that dual‐ferroelastic phase toughening mechanisms effectively enhance the fracture toughness, and thermal conductivity is reduced at the same time, and this work proposes an effective strategy for the design and development of high‐performance TBCs for aero‐engine applications.
No takes yet. Share an insight, caveat, or question.
Shan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: