New stainless steels based on the system Fe‐30Mn‐5AI‐XCr‐0.5C (Cr mass contents of ≤ 9 %) were developed and evaluated as a replacement of conventional AISI 304 steel. The alloys were produced by induction melting and thermomechanically processed to obtain a fine equiaxed microstructure. A typical thermomechanical processing for AISI 300 austenitic stainless steels was used and included forging at 1200°C, rolling at 850 °C and final recrystallization at 1050 °C. A final fully austenitic microstructure with grains of about 150 μm in size was obtained in all the steels. Tensile tests at temperatures ranging from ‐196 to 400 °C showed similar results for the various alloys tested. In accordance with the values for the elongation to fracture, this temperature range was subdivided into three regions. In the temperature range of ‐196 °C to room temperature, elongation to fracture increases with decreasing temperature. At temperatures ranging from 100 to 300 °C, elongation to fracture increases with testing temperature and serrations on the stress‐strain curve were observed. Finally, higher testing temperatures were accompanied by a decrease in ductility. Examination of the microstructures after deformation led to the conclusion that mechanical twinning was the dominant mechanism of deformation at the tested temperatures.
No takes yet. Share an insight, caveat, or question.
Jiménez et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: