Answers are grounded in this paper and cite their sources.
This study investigates the effect of oxygen pressure on the structural-phase state, microstructure, mechanical properties and tribological behavior of Zr(C,N)-based coatings deposited on U8G tool steel by high-velocity oxygen fuel (HVOF) spraying. The coatings were produced at oxygen pressures of 4.0 × 10 5 , 4.3 × 10 5 and 4.5 × 10 5 Pa, while the spraying distance, propane pressure and air pressure were kept constant. Variation in oxygen pressure was found to affect the relative XRD peak intensities, Rietveld-refined phase fractions, diffraction-line broadening parameters, coating thickness, porosity and tribological response. However, since the coatings exhibited differences in thickness, the interpretation of XRD intensity variations was performed with consideration of possible thickness-related effects and substrate contribution. X-ray diffraction and Rietveld refinement indicated the formation of a multiphase Zr(C,N)-based system containing carbonitride, carbide, nitride, oxide and α-Fe phases. The coating deposited at 4.3 × 10 5 Pa showed the most favorable combination of Zr(C,N)-type phase retention, reduced oxide fraction, low apparent cross-sectional porosity and relatively uniform microstructure. Williamson–Hall analysis suggested the largest coherent scattering domain size of approximately 82 nm and the lowest microstrain of approximately 0.30% for this condition, although these values should be considered as comparative estimates due to partial overlap of Zr 2 CN, ZrC and ZrN reflections. SEM/EDS analysis showed that the coating obtained at 4.3 × 10 5 Pa had the most homogeneous distribution of Zr, C and N and relatively low oxygen content. This coating also exhibited the highest microhardness (1826 ± 38.4 HV 0.5 ), the highest apparent pull-off adhesion strength (18.4 MPa) and the lowest friction coefficient (μ ≈ 0.54 ± 0.01). Quantitative wear assessment according to ASTM G99 showed that this coating had the lowest wear volume and specific wear rate among the investigated samples. SEM examination of wear tracks suggested a correlation between oxygen pressure, coating morphology and wear-track features; however, direct post-wear chemical analysis of the tribofilm would be required to confirm the detailed wear mechanisms. Overall, the results indicate that an oxygen pressure of 4.3 × 10 5 Pa provides the most balanced coating characteristics under the investigated HVOF conditions.
No takes yet. Share an insight, caveat, or question.
SKAKOV et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: