Answers are grounded in this paper and cite their sources.
The thermal decomposition of DLP-printed green bodies containing a cross-linked 1,6-hexanediol diacrylate matrix filled with complex oxide powder of a cerium-activated garnet structure (GYAGG:Ce) was investigated. Non-isothermal thermogravimetric measurements were performed under an argon atmosphere at heating rates of 2, 4, 8 and 20 °C/min (four independent measurements for each heating rate). The main mass-loss stage occurs at approximately 350–470 °C. With the increase in the heating rate, the mean DTG peaks shift to a higher temperature: from 387.1 ± 10.3 °C at 2 °C/min to 427.9 ± 15.2 °C at 20 °C/min. The kinetics of thermal decomposition were investigated using isoconversional analysis methods. The apparent activation energy of the main mass-loss peak calculated by the Kissinger method was 200.85 kJ/mol (R2 = 0.99). Gas-phase mass-spectrometric analysis tentatively assigned signals to water, CO, CO2, and acrylate-derived fragments of organic chains. A thermal analysis-guided debinding schedule was developed and experimentally demonstrated, resulting in the production of bulk ceramics with measurable optical translucence (the full transmittance and in-line transmittance were 54.5% and 12%, respectively, for a sample 1.2 mm thick). The absence of large cracks and delamination was observed in both green and brown bodies by scanning electron microscopy.
No takes yet. Share an insight, caveat, or question.
Ermakova et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: