Answers are grounded in this paper and cite their sources.
Hydrophilic nano-Al2O3 was introduced through the aqueous phase into a commercial water-reactive polyurethane at six loadings of 0–5 wt.% and a fixed polyurethane-to-water volume ratio of 1:1. Reaction and foaming measurements were combined with SEM–EDS and FTIR characterization. Recorded temperature maxima ranged from 36.7 to 39.8 °C. Across three experimental batches, mean foaming ratios ranged from 104.2% to 144.2%, without a statistically significant overall loading effect after accounting for batch. Apparent density at the room-temperature cooling endpoint was on average about 11% lower across the modified formulations than for the control. In the selected two-dimensional SEM fields, modified formulations showed smaller apparent pore dimensions and higher areal pore counts. Mean apparent pore diameter was 265.7 µm for the control and 154.7–209.8 µm for the modified formulations. EDS detected local Al-containing signals, while the main FTIR bands showed no pronounced systematic loading-dependent changes. These observations show finer pores in the analyzed sections without a statistically significant overall loading effect on bulk expansion.
No takes yet. Share an insight, caveat, or question.
Xuchen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: