In this study, the fracture toughness KIC of high performance concrete (HPC) was determined by conducting three-point bending tests on eighty notched HPC beams of 500mm×100mm×100mm at high temperatures up to 450∘C (hot) and in cooled-down states (cold). When the concrete beams exposed to high temperatures for 16 hours, both thermal and hygric equilibriums were generally achieved. KIC for the hot concrete sustained a monotonic decrease tendency with the increasing temperature, with a sudden drop at 105∘C . For the cold concrete, KIC sustained a two-stage decrease trend, dropping slowly with the heating temperature up to 150∘C and rapidly thereafter. The fracture energy-based fracture toughness KIC ' was found to follow similar decrease trends with the heating temperature. The weight loss, the fracture energy and the modulus of rapture were also evaluated.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2014) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: