This is the authors' abstract. We don't add key points for this paper.
Bimetallic structures unlock the ability to combine the superior properties of dissimilar alloys within a single component, yet their fabrication remains constrained by the inevitable formation of brittle intermetallic phases at metallurgically incompatible interfaces. This study employed a hybrid wire arc-directed energy deposition (WA-DED) system to manufacture CPTi–SS316L bimetallic structures. ER CuSi-A was introduced as an intermediate bond layer (IBL) between the two alloys, preventing direct Ti-Fe reactions and the associated formation of brittle intermetallic phases at the interface. A customized WA-DED system featuring localized high-purity argon shielding enabled defect-free deposition of the CPTi in an open environment. Two distinct metallurgical interfaces were identified: ROI 1 at the CPTi/ER CuSi-A junction (200 ± 22 μm), and ROI 2 at the ER CuSi-A/SS316L junction (18 ± 9 μm). Stress-relief heat treatment at 480 °C reduced residual stress in the CPTi zone by 77%. The bimetallic specimens achieved compressive yield strengths of 219 ± 6 MPa and 211 ± 8 MPa in the as-printed and heat-treated conditions, respectively, exceeding those of the wrought CPTi Grade 1 and SS316L counterparts by up to 29%. Tensile testing revealed brittle fracture at ROI 1 with an ultimate tensile strength of 182.5 ± 3 MPa. The fabrication of a functional auger screw prototype with a CPTi overlayer on an SS316L core further demonstrated the mechanical reliability and validated industrial applicability of the proposed approach.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Dash et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: