Boron carbide is one of the most promising structural ceramics; therefore its joining to other ceramics and metals is of technological importance. In this study, interface interactions and joints strength were studied in various cases of B4C/Cu based fillers (Cu-9at%B, Cu-4.5at%Ti and Ticusil®). The fillers partially wet B4C (q < 500), but the interface composition and morphology are different. In the B4C/Cu-9at.%B system no new phases are detected at the interface, while the formation of TiB2 takes place in the case B4C/Cu-4.5at%Ti, and a double layer containing TiB2 and TiC is formed at the B4C/Ticusil® interface. The maximal shear stress for B4C/B4C joints breakage was obtained for the Cu-9at.%B brazing alloy which displays partial wetting without the formation of brittle phases at the ceramic/metal interface. This study shows that improved wetting is essential but not sufficient in order to obtain strong bonding between B4C and the fillers examined.
No takes yet. Share an insight, caveat, or question.
Aizenshtein et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: