In this study, a ceria (CeO2) support, synthesized using a hydrothermal method, was decorated with nano-sized Ni-particles using an impregnation method. A micro-tubular solid oxide fuel cell (MTSOFC) was integrated with a corundum tube, in which the Ni-CeO2 (10 wt% Ni) served as the catalyst for partial oxidation (POX). Using propane and air, there was no noticeable deactivation in the MTSOFC over a 48-h period. The maximum power density (MPD) was 0.57 W cm −2 at 700°C using propane and air (12.3 vol% propane), which is 0.01 W cm−2 higher than the cell using 20 vol% of hydrogen (0.56 W cm −2). When using propane and air as fuel and operating at 700°C, MPD values for intermediate and inlet current collector modes were 0.57 and 0.48 W cm−2, respectively. Carbon deposition at the fuel inlet was determined to be the primary cause of low current collection efficiency.
No takes yet. Share an insight, caveat, or question.
Guo et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: