Lanthanum hexaboride (LaB 6 ) is a functional material with excellent thermionic emission and near-infrared (NIR) absorption properties but has typically required the use of temperatures exceeding 1400 °C during synthesis. The present study demonstrates the low-temperature synthesis of LaB 6 powder using a novel method taking advantage of the thermodynamic driving force associated with sodium silicate (Na 2 SiO 3 ) formation. LaB 6 powder was obtained by heating compacts of La 2 O 3 , B 2 O 3 , and SiO 2 powders with Na metal at 600–1100 °C under an argon atmosphere. The large negative standard Gibbs free energy change for the primary reaction (La 2 O 3 + 6B 2 O 3 + 21SiO 2 + 42Na → 2LaB 6 + 21Na 2 SiO 3 ; Δ G ° = −2993 kJ/mol at 1027 °C) allowed the synthesis to proceed at significantly reduced temperatures. By-products such as Na 2 SiO 3 , NaLaSiO 4 , and Na 3 LaB 2 O 6 were easily removed by water washing and subsequent leaching with 2 mol/L HCl, yielding pure LaB 6 powder with particle sizes in the range of tens of nanometers to 3 μm. As the synthesis temperature was increased, the size of the LaB 6 crystallites increased from 12.7 to 142 nm while the lattice strain decreased from 0.145% to 0.015%. Notably, the molten Na 2 SiO 3 (which has a melting point of 1088 °C) acted as a flux at temperatures in the vicinity of 1000 °C to enhance particle growth and promote the formation of well-faceted cubic crystals via a dissolution-precipitation mechanism. The LaB 6 powder synthesized at 1100 °C exhibited NIR absorption originating from localized surface plasmon resonance (LSPR), which was nearly equivalent to that of a commercial LaB 6 powder, demonstrating the practical potential of this material for NIR shielding applications.
No takes yet. Share an insight, caveat, or question.
Yamada et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: