Recycling waste glass as a partial cement replacement is a promising strategy to reduce cement consumption while promoting the valorization of a widely available waste material. This study investigates the reinforcing efficiency of silica/multiwalled carbon nanotube nanocomposites (SiO2/MWCNT) in cement mortars containing 20 wt% waste glass powder (WGP) as a partial replacement for Portland cement (PC). Nanocomposites with SiO2-to-MWCNT mass ratios of 1:99 and 5:95 were incorporated at ultra-low dosages (0.025 wt% of the total binder content). Their influence on hydration, microstructure, aqueous dispersion stability and mechanical performance was evaluated. Results showed that the 1:99 nanocomposite increased compressive and flexural strength by 19.1% and 39.6%, respectively, compared to the WGP mortar. It also surpassed the flexural strength of the reference mortar by 23.8% at 28 days. The lower SiO2-to-MWCNT ratio yielded greater mechanical strengths than the higher one, suggesting that, under the investigated conditions, increasing the SiO2-to-MWCNT ratio does not necessarily improve reinforcement efficiency in silica-rich cementitious systems. These findings highlight the potential of SiO2/MWCNT nanocomposites prepared with a low proportion of SiO2 to compensate for the mechanical limitations associated with waste-glass incorporation, supporting the development of more sustainable cementitious materials with reduced cement consumption.
No takes yet. Share an insight, caveat, or question.
Castro-Botello et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: