Answers are grounded in this paper and cite their sources.
Water droplets formed by the deliquescence of pre-deposited NaCl on 316L stainless steel were investigated. Different total weights of NaCl particles between 0.0005 g and 0.01 g were deposited on 316L stainless steel surface, which were exposed to an atmospheric condition at 80oC and relative humidity of 80% until NaCl droplets were stabilized. The volume of NaCl droplet was linearly proportional to the total weights of pre-deposited NaCl and consequently the chloride concentration in droplets, ranging from 3 to 6 M, did not depend on the NaCl weights. After exposed to the NaCl droplets at 80oC and relative humidity of 80% over 5, 10, and 15 days, all 316L stainless steel samples suffered from pitting. The Cl- ions in the surface films of samples were measured by ToF SIMS. The pit densities on samples were well correlated with the Cl- intensities in the surface films. These results suggest that the pit initiation under NaCl droplets by deliquescence is caused by the Cl- ions either incorporated into surface films or penetrated through them.
No takes yet. Share an insight, caveat, or question.
Mehrzi et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: