This study investigated the near-full densification of pure aluminium (Al) powder through Electromagnetic Radial Powder Compaction (EMRPC). Experiments were performed at discharge voltages of 11 kV, 12 kV, and 13 kV. Field-shaper was used as tool and the field shaper enhanced the magnetic flux density at the tube-field shaper interface by a factor of approximately 2. Vickers’ micro-hardness tests were performed, and optical microscopy was used to check the structure at the microscopic level. These results demonstrate that EMRPC with a copper driving tube and field shaper constitutes an effective and rapid densification strategy for aluminium powder, yielding near-theoretical density compacts within microseconds. The maximum relative density of 98.5% (2.66 g/cc) and the peak tube velocity were 75.8 m/s achieved at 13 kV discharge voltage. A loosely coupled finite element simulation using ANSYS Maxwell and LS-DYNA was developed and experimentally validated. As the discharge voltage increased from 11 kV to 13 kV, the optical microstructure of the compacted aluminium samples progressively became denser and more homogeneous, with reduced inter-particle porosity and more intimate particle-particle bonding, confirming the microstructural basis for the observed improvements in density and hardness.
No takes yet. Share an insight, caveat, or question.
Thirupathi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: