Spherical Fe- and Ti-modified mesoporous MCM-41 materials were prepared and investigated as photocatalysts for CO 2 reduction at pH 7 and 12.9. Characterization confirmed the preservation of the ordered mesoporous structure and high specific surface area, while revealing differences in surface composition, Ti species, and photoelectrochemical properties. The highest photocatalytic activity at pH 12.9 was achieved by 20Fe-S-MCM-41, with a total yield of CO 2 reduction products (CH 4 + CO) of 25.4 μmol g cat −1 , including 25.3 μmol g cat −1 of CH 4 , whereas the bimetallic 2.5Fe-5Ti-S-MCM-41 exhibited the highest activity at pH 7 (17.2 μmol g cat −1 , comprising 13.3 μmol g cat −1 of CH 4 and 3.9 μmol gcat −1 of CO) and the second-highest activity at pH 12.9. The differences in photocatalytic performance could not be explained solely by the nominal Fe and Ti contents but were associated with variations in surface composition, the nature of metal species, and photoelectrochemical behavior. Alkaline conditions significantly enhanced the formation of CO 2 reduction products and the electron-based selectivity toward CO 2 reduction for all investigated materials, whereas competing H 2 evolution was more pronounced at pH 7. This behavior likely reflects the combined influence of pH-dependent inorganic carbon speciation and competition between CO 2 reduction and H 2 evolution. The results demonstrate that both photocatalyst composition and reaction pH must be considered when optimizing photocatalytic CO 2 reduction activity and selectivity.
No takes yet. Share an insight, caveat, or question.
Jablunka et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: