Initially anode-free Li-metal batteries, in which Li-metal is constructed in-situ during charging, enable increased energy density. However, interfacial degradation reactions between the electrolyte and lithiophobic Cu prevent stable solid electrolyte interphase formation on the negative electrode. Here, we elucidate a time-evolving interfacial mechanism in which adsorption of electrolyte components contributes to initial interfacial layer formation and solid electrolyte interphase stability. Most organic solvents adsorb more strongly than Li-salt compounds on Cu through van der Waals dispersion interactions. This preferential adsorption produces a solvent-dominated interfacial layer that undergoes rapid compositional reconstruction during Cu oxide reduction upon initial charging. In contrast, lithium tetrafluoroborate possesses a tetrahedral anion with isotropic charge distribution that binds strongly to the Cu (111)/(100) surfaces and native Cu oxides, producing a tetrafluoroborate-driven interfacial layer that electronically passivates the Cu interface and promotes homogeneous Li nucleation. Consequently, lithium tetrafluoroborate-containing cells achieve 62% capacity retention after 300 cycles at an areal capacity of 4.1 mAh cm−2 and electrolyte conditions of 1.5 g Ah−1 and 4 μL cm−2, establishing a mechanistic basis for adsorption-driven interfacial design in initially anode-free Li-metal batteries. Initially anode-free lithium-metal batteries are limited by unstable interfacial reactions at Cu current collectors. Here, authors show that preferential anion adsorption can stabilize the copper interface and improve long-term cycling.
No takes yet. Share an insight, caveat, or question.
LEE et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: