Antimony trisulfide (Sb2S3) is a promising quasi-1D absorber for tandem photovoltaics, sensors, and self-powered indoor Internet-of-Things (IoT) electronics, yet its multifaceted deep-level defect landscape limits device performance. Here, we precisely modulate the post-deposition thermal crystallization dynamics of open-air, ultrasonic spray-deposited Sb2S3 thin films at 300 °C to decouple bulk defect passivation from interfacial thermal degradation. Extending post-deposition crystallization time from 6 to 12 min mitigates dominant non-radiative Shockley-Read-Hall recombination, yielding an order-of-magnitude reduction in reverse saturation current density (J0) and decreasing the light-intensity-dependent ideality factor (A) from 1.61 kBT/q to 1.31 kBT/q. Deep-level transient spectroscopy (DLTS) and space-charge-limited current (SCLC) analyses reveal that optimized 12 min annealing duration drastically reduce the inverse capture mean free path or recombination strength (σNT) of both deep and shallow defects. This thermal annealing process involves competing physical mechanisms; prolonged thermal exposure to 18 min triggers sublimation-induced film thinning of the Sb2S3 absorber, compromising back-contact interfacial quality. Consequently, the optimized 12 min device yields a remarkable efficiency of 6.12 % with an outstanding VOC of 718 mV, whereas the 18 min counterpart underperforms despite a higher VOC of 734 mV. This work demonstrates a viable pathway for optimizing thermal processing parameters in low cost, solution-processed, and scalable open-air Sb2S3-based optoelectronics.
No takes yet. Share an insight, caveat, or question.
Asare et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: