Answers are grounded in this paper and cite their sources.
To simultaneously tackle the pronounced autogenous shrinkage and high early-age cracking susceptibility of ultra-high-performance concrete (UHPC), pre-wetted high-strength coal gangue lightweight aggregate (CLWA) was used as an internal curing agent, completely replacing quartz sand to fabricate reduced-density UHPC. The results indicate that incorporating CLWA not only maintained adequate workability but also reduced the density of the UHPC by 15.4% to 2250 kg/m3, while achieving a 28-day compressive strength of 117 MPa. More importantly, the use of CLWA resulted in remarkable internal curing efficiency, reducing the 60-day autogenous shrinkage by 51.5% and the chloride migration coefficient by 60%. Furthermore, no detectable carbonation depth was observed after 56 days of exposure. Microscopic analysis further indicated that the slow water-release characteristics of CLWA promoted sustained hydration and were associated with a more favourable composite pore-size distribution (with the combined fraction of pores below 50 nm reaching 38.0%) and a denser, locally stronger aggregate–paste interfacial region, collectively underpinning the improved macro-performance of UHPC. A multi-scale relationship between the water-storage/release characteristics of CLWA, pore and interfacial transition zone evolution, and the resulting shrinkage and durability performance of UHPC was established.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: