Waste lithium aluminosilicate (LAS) glass is a complex secondary resource characterized by high aluminum and high silicon content, posing significant challenges for the selective recovery of lithium. Conventional recycling processes for such materials are often hindered by poor separation selectivity, complex purification steps, and high energy consumption. To address these limitations, this study proposes an integrated process comprising mixed sulfate roasting, water leaching, selective magnesium precipitation, and lithium carbonate crystallization. Under optimal conditions with a mass ratio of m(K2SO4):m(Na2SO4):m (raw material) = 0.5:0.5:1, roasting at 900 °C for 120 min resulted in the conversion of over 97% of lithium into water-soluble lithium-containing sulfate phases, while aluminum and silicon were transformed into insoluble phases, specifically KAlSi2O6 and Na (AlSi3O8). Subsequent water leaching enabled the direct separation of lithium without the use of acids or alkalis. After roasting and water leaching, a lithium leaching efficiency of 97.19% was achieved, whereas the leaching efficiencies of aluminum and silicon were both below 0.01%, demonstrating exceptional separation selectivity. Residual magnesium impurities in the lithium-bearing leachate were effectively removed via sodium hydroxide precipitation. At an optimized pH of 10.18, the magnesium removal efficiency reached 99.05%. Following purification, lithium carbonate was recovered by sodium carbonate precipitation at 95 °C for 60 min, yielding a Li2CO3 precipitation recovery of 95.33%. Based on these stages, the actual overall lithium recovery of the entire process was calculated to be 92.68%. Compared with conventional LAS-processing routes (salt roasting and acid leaching, or CaO-based calcination generating large amounts of solid waste), this process uses only deionized water for leaching, eliminating acid or alkali consumption. Relative to the conventional spodumene route (1100 °C phase transformation + acid or alkali leaching), the roasting temperature is lowered by 200 °C to 900 °C. This novel process offers a sustainable and economically viable pathway for lithium recovery from waste LAS glass, characterized by reduced energy consumption, minimized environmental impact, and enhanced resource utilization.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: