Purpose This study aims to develop a sustainable cement mortar incorporating post-industrial textile waste fibres and evaluate long-term performance, together with the underlying mechanisms governing the behaviour. Design/methodology/approach Waste textile fibres (cotton, polyester, nylon and elastane) were incorporated into cement mortars and evaluated at 28, 90, 180 and 365 days to assess thermal conductivity, sound absorption, compressive strength and drying shrinkage. Microstructural characterisation using scanning electron microscopy (SEM), micro-computed tomography (Micro-CT) and nanoindentation was conducted to investigate microstructure, pore structure and interfacial transition zone (ITZ) behaviour of fibre-reinforced cement mortars (FRMs). A multicriteria decision-making approach based on the Simple Additive Weighting (SAW) method was applied to rank the mix formulations in terms of thermal, acoustic, compressive strength and shrinkage performance. Findings The overall best-performing ELS FRM achieved the lowest thermal conductivity (0.8 W/mK), around 38% higher average sound absorption than the control, a compressive strength of 49 MPa and approximately 10% lower total shrinkage compared to the control at one-year age. Porosity analysis revealed that ELS FRM exhibited the highest total porosity among all mixes, governed primarily by the high elasticity and fibre geometry of elastane, which can promote air entrapment during mixing and lead to increased internal void content. Despite this porous structure, the high elasticity and deformation compatibility of elastane fibres govern improved stress redistribution and crack-bridging within the matrix, thereby maintaining compressive strength and reducing shrinkage. Originality/value This research addresses key limitations in existing FRMs by furthering the scarcity of studies extending beyond early ages (7–90 days) and the lack of coupled long-term datasets linking thermal, acoustic, compressive strength and shrinkage performance. In addition, this study develops a clearer understanding of the underlying mechanisms governing performance by addressing the limitation that most existing studies rely on isolated testing ages and SEM observations, without integrated characterisation of microstructure, porosity and ITZ properties. This paves the way for scalable FRM production and practical use in non-load-bearing applications subject to further validation under real exposure conditions.
No takes yet. Share an insight, caveat, or question.
Wijesinghe et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: