Answers are grounded in this paper and cite their sources.
Brick waste from construction and demolition is predominantly crystalline and develops little strength when alkali-activated at room temperature. This study examined whether the controlled addition of Portland-composite cement (PC) can overcome this limitation. Ground brick powder was activated with NaOH and colloidal silica, and the PC/binder mass ratio (10–40 wt.%), Na2O/binder mass ratio (1.5–6.0 wt.%) and SiO2/Na2O molar ratio (0.50–1.25) were varied according to a Taguchi L16 design. PC content was the dominant factor for 7-day compressive strength, followed by the SiO2/Na2O ratio, whereas the Na2O dosage had no significant effect on strength. The mixture with the highest predicted strength within the investigated range reached 12.41 MPa at 7 days and 19.3 MPa at 90 days under ambient curing, 9.6 and 4.5 times the strength of the brick-only reference, while a low-alkali mixture (1.5 wt.% Na2O) achieved a comparable strength. Curing at 60 °C gave 17.2 MPa at 7 days. Flow was governed mainly by the Na2O dosage, and all tested hybrid pastes set much faster than the reference binders. Calorimetry, thermogravimetry and X-ray diffraction were consistent with greater reaction-product formation than in the brick-only binder. The strengths achieved point to non-structural applications, such as masonry mortars and precast elements.
No takes yet. Share an insight, caveat, or question.
Kioupis et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: