Answers are grounded in this paper and cite their sources.
The combined effects of low AlSi12 additions on densification, mechanical properties and load-dependent wear in bulk NiCrBSi consolidated by spark plasma sintering (SPS) remain insufficiently established. This study evaluates AlSi12 as a metallic modifier to improve hardness and wear resistance while identifying associated flexural-strength trade-offs. Compositions containing 0, 2, 4, 6 and 8 wt.% AlSi12 were processed at 950 °C under 38 MPa for 240 s in nitrogen. Phase constitution, microstructure, density, hardness, bending strength and dry-sliding wear at 50 and 100 N were examined. The Ni-rich matrix remained dominant, with local Al enrichment. Experimental density decreased from 8.01 to 6.97 g/cm3, whereas nominal relative density was highest, at approximately 98.7–98.9%, for 4–6 wt.% AlSi12. The highest reported mean hardness was 581 HV at 6 wt.%, while the unmodified alloy reached the highest maximum nominal flexural stress in the displayed bending records. The lowest specific wear rates were approximately 2.6 × 10−5 and 2.9 × 10−5 mm3/(N·m) for 6 wt.% at 50 N and 8 wt.% at 100 N, respectively. These findings support composition selection based on the required balance of hardness, flexural strength and load-specific wear resistance.
No takes yet. Share an insight, caveat, or question.
Çelik et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: