The microstructural and mechanical evolution of powder metallurgy-processed Mg–6Zn across a size-adjusted sintering and hot extrusion sequence was investigated. The sintered alloy showed higher EDX Zn intensity near the original Mg particle peripheries and lower intensity toward their interiors, consistent with inward Zn redistribution during two-step sintering. The subsequent processing sequence, comprising the longer billet size-adjusted second-stage hold, a 5 min hold at 300 °C, and hot extrusion, produced a nearly fully dense, fine-grained material with a comparatively uniform Zn distribution pattern at the spatial resolution of EDX mapping. Grain size was refined from 22.08 μm (sintered) to 4.23 μm (extruded). Estimated porosity decreased from 3.40% to approximately 0.11%, indicating substantial consolidation. XRD and SEM did not detect elemental Zn or Mg–Zn intermetallic phases in the sintered and extruded conditions. The extruded Mg-6Zn alloy achieved an ultimate compressive strength of 458 MPa with a work of fracture of 57.2 MJ/m3. Under tension, the extruded Mg-6Zn alloy achieved a tensile yield strength of 202 MPa and ultimate tensile strength of 311 MPa, with a failure elongation of 19.4%. Fractographic analysis revealed a transition from prior particle boundary and faceted fracture in the sintered alloy to predominantly dimpled fracture in the extruded alloy, indicating local plastic deformation during fracture. These results demonstrate that the complete powder processing and hot extrusion route effectively consolidates the diffusion-alloyed Mg–6Zn alloy and produces a refined microstructure with a competitive strength–ductility combination.
No takes yet. Share an insight, caveat, or question.
Hassan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: