Residual stresses and the resulting distortion remain major challenges in achieving high dimensional accuracy in laser beam powder bed fusion (PBF-LB) components. This study experimentally investigates the distortion behavior of PBF-LB cantilever specimens fabricated from IN718 and Ti6Al4V, with particular emphasis on the effects of scan strategy and stress-relief heat treatment. Three hatch rotation angles (31°, 45°, and 90°) were evaluated under as-built (AB) and stress-relieved conditions using 3D optical scanning measurements obtained before and after wire electrical discharge machining (EDM) separation. The AB specimens exhibited progressive deformation along the cantilever length, with Ti6Al4V developing approximately twice the distortion measured for IN718. The 90° hatch strategy produced the highest distortion, whereas 31° and 45° strategies resulted in lower deformation levels. Stress-relief heat treatment proved to be the dominant factor, reducing distortion by 94–97% and substantially decreasing the influence of hatch rotation.
No takes yet. Share an insight, caveat, or question.
Bucaciuc et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: