Answers are grounded in this paper and cite their sources.
The crystallinity of β-Ga2O3 thin films grown by metal–organic chemical vapor deposition (MOCVD) is strongly influenced by reactor design. We investigate the effect of reactor height on crystallinity in MOCVD-grown β-Ga2O3 films by directly comparing long- and short-chamber showerhead configurations. The β-Ga2O3 films were grown heteroepitaxially on c-plane α-Al2O3 (0001) substrates with the (−201) orientation for 40 min at a growth rate of approximately 1 μm/h. Structural evolution was probed by high-temperature x-ray diffraction (HT-XRD) during heating from 25 to 1100 °C. Temperature-dependent XRD reveals a systematic red shift of the β-Ga2O3 (−201) reflection toward lower 2θ upon heating for both reactor geometries, followed by a blue shift toward the initial position upon cooling, consistent with a largely reversible, thermally driven lattice-expansion response. Temperature-dependent rocking-curve analysis reveals distinct FWHM evolution for the two films: the short-chamber film decreases from approximately 2.83° at 25 °C to ∼2.65° at 500 °C before broadening to ∼2.85° at 1100 °C, whereas the long-chamber film broadens from approximately 2.07° to ∼2.38° over the same temperature range; after cooling, the respective FWHM values recover to approximately 2.72° and 2.03°. Atomic force microscopy shows smoother short-chamber films, with root-mean-square roughness decreasing from 7.7 to 7.3 nm after HT-XRD heating, compared with 19.3–12.3 nm for long-chamber films. Overall, these results indicate that reactor height influences the initial crystalline and morphological templates of β-Ga2O3 films and modulates their elevated-temperature structural response, providing practical insights into optimizing MOCVD reactor design for high-quality β-Ga2O3 growth.
No takes yet. Share an insight, caveat, or question.
Rahaman et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: