This study employs a co-precipitation method to synthesize ZnFe2-xMnxO4 (ZFO_Mn_x) anode materials for lithium-ion batteries. Precursors including ZnCl2 and Fe(NO3)3.9H2O were doped with MnCl2 at three molar ratios (x = 0.1, 0.2, and 0.3), with the solution pH strictly controlled at 11 using NaOH. The obtained precipitates were subsequently calcined at 750 °C for 3 h to form the spinel phase, denoted as ZFO_Mn_0.1, ZFO_Mn_0.2, and ZFO_Mn_0.3, respectively. Structural and morphological characterizations using X-ray diffraction and field-emission scanning electron microscopy reveal that a secondary Fe2O3 phase emerges within the spinel matrix at a Mn doping level of x = 0.2. The synthesized materials exhibit high crystallinity and uniform morphology, with particle sizes in the range of 30–40 nm. Electrochemical measurements show that all three electrodes deliver an exceptionally high initial charge capacity, exceeding 751.38 mAh g⁻¹. Among them, the ZFO_Mn_0.2 electrode exhibits superior cycling stability, retaining a reversible capacity of 783.53 mAh g⁻¹ along with the lowest charge-transfer resistance. This outstanding performance is primarily attributed to the optimal proportion of the secondary Fe2O3 phase, which forms a robust multiphase nanocomposite capable of buffering volume expansion and facilitating charge-transfer kinetics. These findings indicate that optimizing the Mn doping concentration, thereby controlling the secondary phase formation, is an effective strategy for improving both the structural durability and electrochemical performance of lithium-ion battery anodes.
No takes yet. Share an insight, caveat, or question.
Nguyen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: