Flexible WO3 electrochromic films require interfaces that facilitate reversible Li+ insertion/extraction while maintaining stability during repeated cycling. Here, ultrathin Al2O3 interfacial layers were deposited on WO3/ITO/PET electrodes by low-temperature atomic layer deposition (ALD) using 3, 5, and 10 cycles. Increasing the ALD cycle number progressively suppressed the initial electrochemical response and apparent Li+ transport kinetics. Nevertheless, the 3- and 5-cycle samples exhibited improved cycling durability, retaining optical modulation (ΔT) values of 55.97% and 54.48% after 150 cycles at room temperature, corresponding to 90.6% and 88.0% of their initial values, respectively, compared with a decrease from 64.18% to 20.32% for pristine WO3. In contrast, the 10-cycle sample exhibited activation-like behavior, with ΔT increasing from 31.72% to 59.08% within 150 cycles, although its long-term stability remains uncertain. Combined optical, electrochemical, and XPS analyses suggest a thickness-dependent, non-monotonic interfacial effect, balancing ionic accessibility and cycling stability at lower ALD loadings while inducing initial kinetic restriction and subsequent electrochemical conditioning at higher loading. These findings highlight the potential of ALD-derived Al2O3 interfacial layers for tailoring the electrochromic performance of flexible WO3 films.
No takes yet. Share an insight, caveat, or question.
Chu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: