A flux-free low-temperature soldering method using liquid Ga pre-coating was proposed to realize reliable joining of 6063Al/Cu dissimilar metals with SAC305 solder in air. Thin Ga layers were coated on both substrates at 30 °C, followed by assembling a 6063Al/SAC305/Cu sandwich structure and soldering at 250 °C with holding times of 10 s, 30 s and 60 s. Interfacial microstructure, elemental distribution, shear strength and large-area bonding performance were systematically characterized. Liquid Ga effectively broke the dense native oxide films on the 6063Al and Cu surfaces and promoted uniform elemental interdiffusion across the joint. The typical intermetallic compounds formed at Cu/solder and Al/solder interfaces, which thickness and morphology were governed with holding time. The joint with 30 s holding exhibited the optimal shear strength of 56–61 MPa, attributed to continuous and crack-free moderate-thickness intermetallic layers. Insufficient diffusion at 10 s induced incomplete reaction layers and moderate strength, while excessive holding at 60 s caused severe coarsening of brittle intermetallic and interfacial microcracks, reducing mechanical performance. Fracture path propagated entirely along brittle Cu–Al intermetallic layers. Furthermore, sound 45 mm × 45 mm large-area joints without macroscopic defects were successfully fabricated, verifying the great application potential of this Ga-assisted soldering technique for large-size electronic packaging dissimilar components.
No takes yet. Share an insight, caveat, or question.
Wu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: