BiTe‐based room‐temperature thermoelectric (TE) material family suffers from intrinsic efficiency‐limiting carrier‐mobility trade‐offs. Herein, we report an n‐type Bi 0.75 Sb 0.25 Te 0.7 S 0.15 Se 0.15 material with tailored local compositional fluctuations, which achieves a peak ZT of ∼ 0.64 at 377 K and a record‐high average ZT ave of ∼0.56 over 300–573 K, which stands as the maximum value for BiTe‐based TE systems. The excellent performance originates from conduction band flattening and dense intragranular dislocations, which are produced by the local compositional fluctuations. Band flattening spanning the Γ–A path together with enhanced valleys alignment increase the carrier effective mass, thereby improving the Seebeck coefficient. In addition, intragranular dislocations induce multiscale stress mismatches to achieve efficient phonon scattering, while reducing lattice elastic deformation and weakening phonon‐electron coupling. These synergistic effects allow this alloy a high power factor of ∼14.7 µW cm −1 K −2 and a low lattice thermal conductivity of 0.37 W m −1 K −1 at 377 K. This work proposes a feasible and effective strategy for modulating charge and phonon transport in TE materials.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: