Answers are grounded in this paper and cite their sources.
To improve the comprehensive mechanical properties of FexCrNi(AlTi)0.2 medium-entropy alloys, laser melting deposition (LMD) was employed as the fabrication method. By varying the Fe content, the effects of Fe concentration on the microstructure, mechanical properties, and corrosion resistance of FexCrNi(AlTi)0.2 (x = 1, 2, 3, 4, and 5) medium-entropy alloys were systematically investigated. The results indicate that the fraction of the BCC phase gradually decreases with increasing Fe content. In particular, the Fe5 alloy exhibits a high density of fine BCC precipitates within the FCC grains. Furthermore, the tensile yield strength at room temperature decreases with increasing Fe content, and a similar trend is observed in a 3.5 wt.% NaCl solution. Within a certain Fe content range, increasing the Fe content effectively improves the elongation at fracture. Among the investigated alloys, Fe2 exhibits the best comprehensive mechanical performance, with yield strengths of 837 ± 10 MPa at room temperature and 845 ± 14 MPa in a 3.5 wt.% NaCl solution. The corresponding elongations at fracture are 41.8 ± 0.5% and 30.9 ± 0.5%, respectively, indicating relatively stable mechanical performance under different environments. In addition, the resistance of the alloys to both uniform and localized corrosion gradually decreases with increasing Fe content. Nevertheless, spontaneous passivation occurs in the 3.5 wt.% NaCl solution, resulting in the formation of a protective passive film.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: