Quartz-rich iron ore tailings represent a potential secondary source of silica, although residual impurity-bearing phases may limit purification by conventional separation routes. This study investigated the influence of microwave irradiation on the upgrading of iron ore flotation tailings through magnetic separation and subsequent mixed-acid leaching. Microwave treatments were performed at 700, 1100, and 1600 W under different irradiation times, with and without water quenching. The most pronounced microstructural changes were obtained at 1600 W for 6 min. BET specific surface area increased from 1.1382 m 2 /g in the feed to 2.7302 m 2 /g without quenching and 1.8437 m 2 /g with quenching, while SEM revealed micrometre-scale cracks without detectable mineralogical transformation. After ultrasound-assisted staged magnetic separation up to 1.0 T, the selected products contained 91.93 and 90.73 % SiO 2 , respectively. Their response to acid leaching was enhanced compared with the untreated control, with Fe removal reaching 99.8 and 99.7 %, accompanied by high removals of Al, K, and Mg. After two leaching stages, SiO 2 contents reached 99.76 and 99.82 %, increasing to 99.92 and 99.91 % after a third stage. Residual Fe concentrations decreased to 76 and 141 ppm, respectively, while XRF independently indicated 99.94 % SiO 2 for both final products. XRD confirmed α-quartz as the predominant crystalline phase, and SEM–EDS showed only sparse residual Fe- and Al-rich regions.
No takes yet. Share an insight, caveat, or question.
Fonseca et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: