This study investigates the degradation mechanisms of ordinary portland cement (PC) and portland–limestone cement (PLC) pastes under continuous exposure to sulfuric and acetic acids. Paste specimens ( w / c = 0.40 ) were immersed for 90 days in 0.1 M H 2 SO 4 and 0.5 M CH 3 COOH , with solutions renewed every 10 days. Deterioration was quantified by mass change, residual compressive strength, depth of alteration, bulk electrical resistivity, formation factor, pore-solution chemistry, and phase analyses. In sulfuric acid, both binders initially gained mass through gypsum and ettringite precipitation before transitioning to net loss after rim disintegration. After 90 days, PC lost 11.6% of its mass and retained 56% of its original strength, whereas PLC lost 4.1% and retained 25%. In acetic acid, both experienced nearly linear mass loss of 26%, with strength retention of 41% for PC and 20% for PLC. Bulk resistivity and the formation factor both rose temporarily and then declined in sulfuric acid, consistent with alternating rim formation and failure, and both decreased monotonically in acetic acid, indicating uninterrupted leaching and decalcification. X-ray diffraction (XRD) and thermogravimetric analysis (TGA) results corroborated these mechanisms through the detection of gypsum as the dominant sulfate-attack product and calcium-acetate hydrates under acetic acid exposure. The results show that at paste scale and under continuous exposure, PLC delayed surface loss but developed deeper altered rims and lower residual strength once its buffering capacity was depleted.
No takes yet. Share an insight, caveat, or question.
Tuaum et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: