The photocatalytic performance of TiO2 powders is commonly associated with specific surface area, crystallite size, and phase composition; however, the extent to which these characteristics remain relevant after incorporation into cementitious materials is not well established. This study investigated nine commercial TiO2 photocatalysts spanning BET surface areas of 53.8–360.6 m2/g. The powders were physicochemically characterized and evaluated for NOx abatement, after which seven representative photocatalysts were incorporated into cement mortars at dosages of 4–18 kg/m3 and tested for NOx removal and self-cleaning performance. At the powder scale, NO removal generally increased with BET surface area, although the improvement diminished above approximately 200–240 m2/g. Incorporation into mortar fundamentally altered this relationship. P25, despite having the lowest BET surface area and powder-scale NO removal, exhibited the highest mortar-scale activity, exceeding 220 μg/(m2·h), whereas high-BET photocatalysts generally remained below 80 μg/(m2·h). DLS and SEM/EDS analyses indicated that composite-scale performance was more closely associated with photocatalyst accessibility after hydration than with nominal powder surface area or agglomerate size alone. Two complementary indicators were therefore introduced: the Photocatalytic Utility Index (PUI), quantifying overall powder-to-composite performance transfer, and the Dose–Response Index (DRI), quantifying response to increasing photocatalyst content. Low-BET photocatalysts exhibited substantially higher PUI and DRI values than high-BET materials.
No takes yet. Share an insight, caveat, or question.
Jackiewicz-Rek et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: