Low-temperature Cu–Cu bonding is essential for high-density three-dimensional integration because excessive thermal budgets can cause wafer warpage, bonding misalignment, and back-end-of-line reliability issues. In this study, Ar, N2, and O2 plasma treatments were applied for 10 and 30 s to Cu surfaces passivated with an approximately 7 nm-thick electroless-plated Au nanolayer. The effects on surface composition and roughness were evaluated using X-ray photoelectron spectroscopy (XPS) and atomic force microscopy (AFM), followed by Cu–Cu bonding at 200 °C and 15 MPa. Bonded interfaces and mechanical strength were examined using transmission electron microscopy (TEM) and die shear testing. All plasma treatments reduced surface carbon contamination. Ar treatment decreased the near-surface Au signal and increased the Cu signal, without uniquely establishing Au-layer thinning. N2 treatment exhibited low surface oxygen, whereas O2 treatment produced greater oxygen-related XPS signals. After 30 s, roughness increased in the order N2 (6.463 nm) < O2 (8.484 nm) < Ar (10.14 nm). Mean shear strengths among successfully bonded specimens were 16.21, 15.90, and 10.56 MPa, respectively, while specimen-level bonding success rates were 75% (15/20), 35% (7/20), and 50% (10/20), respectively. Under the investigated, non-identical plasma processing conditions, N2 yielded the lowest measured roughness and the highest observed bonding success rate.
No takes yet. Share an insight, caveat, or question.
Go et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: