This study aims to investigate the effect of titanium dioxide (TiO 2 ) nanoparticles on the mechanical and physical properties of polymethyl methacrylate (PMMA)-based acrylic composite materials suitable for temporary dental applications. The samples were prepared using Orthocryl resin with 0, 1, 3, 5, 7, and 10 wt.% TiO 2 added via a mold pressing technique. Tensile strength, elongation, elastic modulus, toughness, fracture toughness, hardness, wear resistance, density, water absorption, FESEM analysis, and FTIR analysis were investigated. Results showed that the enhancement in mechanical properties due to the increase of TiO 2 concentration up to 7 wt.% is noticeable. The tensile strength rises from around 17 MPa for pristine material to about 41 MPa for 7 wt. % TiO 2 , elongation increases from around 1.3% to 3.5%. Elastic modulus increases from around 1.1 GPa–2.1 GPa for 10 wt. % TiO 2 , hardness increased from around 55 to 73 Shore D. Toughness increased from around 3.7 to 7.1 J/m 2 for 7 wt.% TiO 2 , and fracture toughness increased from around 0.06 to 0.14 MPa·m 1/2 for 10 wt.%. Furthermore, wear rate reduced with an increase in TiO 2 concentration in the 5–7 wt.% range, but density rose from 1.10 to 1.165 g/cm 3 and water absorption from 3.3% to 4.9%. FESEM analysis showed denser and more uniform microstructure of samples in case of moderate TiO 2 concentration, whereas FTIR spectrum did not reveal any changes in chemical structure of acrylic resin matrix. In general, 7 wt.% TiO 2 proved to be optimal for mechanical and tribological characteristics.
No takes yet. Share an insight, caveat, or question.
Oleiwi et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: