In this study, AISI H13 hot-work tool steel is pack boronized at 900 and 950°C for 2–4 h using a 70% SiC-20% B 4 C-10% KBF 4 powder mixture. Cross-sectional SEM-EDS analyses show a continuous saw-tooth boride layer with a strong boron gradient. The layer thickness ranges from 22 to 50 µm; at 900°C it rises from 24.5 to 45.5 µm when the duration increases from 2 to 4 h (85.7%), while at 950°C it increases from 31.5 to 50 µm (58.7%). At constant duration, raising the temperature from 900°C to 950°C increases thickness by 28.6% at 2 h but only 9.9% at 4 h, indicating diffusion-rate dominance at shorter times and alloying-element barrier effects at longer times. Microhardness values reach 985–1460 HV0.01 at 0.05 mm and decrease gradually to 333–520 HV0.01 at 0.2 mm. Dry sliding tests show a 13.8%–30% reduction in friction relative to the reference (μ avg = 0.80). Tribocorrosion tests reveal a drop in I corr from 22.720 to 1.756–6.323, with the lowest value at 900°C–4 h. Tensile tests at 300°C show significant increases in yield (577 → 987–1366 MPa) and ultimate strength (614 → 1123–1765 MPa), while Charpy impact energy decreases markedly. The results highlight the need to balance boride layer growth with brittleness.
No takes yet. Share an insight, caveat, or question.
Tekaslan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: