This study presents preliminary petrographic screening of four cleaned Üzülmez hard-coal samples from Zonguldak, Türkiye, and three imported steam coals for conceptual cokemaking blend design. No binary blends were prepared or carbonized. Domestic analyzes indicate vitrinite contents of 68–82 vol.%, mean random vitrinite reflectance of 0.97–1.15%, and Free Swelling Index values of 7.5–8.0. Imported samples K1–K3 have lower mean reflectance (0.610–0.771%) and dry-basis volatile matter of 22.18–32.49%. Incomplete petrographic totals and an undefined legacy semi-inertinite category are retained without normalization. Twelve hypothetical compositions containing 20, 30, or 40% imported coal on a dry-mass basis are evaluated using descriptive indices and chemical benchmarks. For Nasifoğlu–K1, the vitrinite-label index decreases from 78.84 to 75.68 and the reflectance index from 1.044 to 0.937% between 20 and 40% addition. These indices summarize input sensitivity. Dry-basis component analyzes enable numerical volatile-matter, ash, and sulfur calculations: sulfur decreases in all four families, whereas volatile matter increases in K1 pairs and decreases in Sulu–K3 and Piç–K2. Imported ash remains approximate, and volatile-matter additivity requires experimental verification. Comparisons with recent studies highlight the importance of interpreting rank and constituent contrasts alongside rheology and charge preparation. The resulting screening matrix identifies compositional trade-offs for subsequent rheological assessment and controlled carbonization.
No takes yet. Share an insight, caveat, or question.
Sarıhan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: