GH4738 superalloy turbine blades easily fail under extreme service conditions. To improve remanufacturability and avoid exclusive reliance on homologous repair materials, GH4169 powder was adopted for laser deposition repair (LDR). A line energy density window of 100–150 J/mm was determined to suppress pores and cracks at the GH4169/GH4738 interface and form sound metallurgical bonding. An improved aging heat treatment (IAHT) was further used to tailor metastable microstructures in the deposited region. IAHT facilitates γ′/γ″ precipitation, partially dissolves brittle Laves phase, and converts some columnar grains into equiaxed grains. After IAHT, macroscopic residual stresses in the substrate, interface and repair zone drop by 34.55%, 46.82% and 42.57%, while intragranular micro-strain (GOS) decreases by 20.95%, 24.88% and 30.62%. The microhardness of the repair zone rises from 247.26 HV0.2 to 443.61 HV0.2. This integrated route enables high-performance blade repair using non-homologous feedstock.
No takes yet. Share an insight, caveat, or question.
Xin et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: